This book was created from invited lectures and conference contributions of the "Metallography & Fractography 2022" conference, which is featured as an essential event for the presentation of results achieved in materials science and engineering. The conference participants come from universities, academic research institutions and different branches of industry with an interest in materials science and engineering. The conference also has strong support from companies that are experts in unique experimental equipment. The conference's ambition is regularly to expand the program to cover new approaches, new advanced materials and technologies, new findings in fundamental research and practical production, and to intensify international contacts.

Les mer

Selected peer-reviewed extended articles based on abstracts presented at the 18th International Symposium on Metallography, Fractography and Materials Science (2022)

Aggregated Book

Les mer
  • Preface
  • Invited Lectures
  • Development of Materials for Solid State Hydrogen Storage
  • Slag from Modern Copper Production Found in Bergwerk, Burgenland, Austria
  • Influence of Surface Machining on Development of Stress Corrosion Cracking of Distribution Wheels of Main Circulation Pump in Nuclear Power Plants
  • Chapter 1: Microstructure, Properties and Processing of Structural Materials
  • Processing and Mechanical Properties of (Hf-Ta-Zr-Nb-Ti)C
  • Application of Composite Filament with the Addition of Metallic Powders in 3D Printing
  • Highly Accurate Structural Analysis of Austempered Ductile Iron Using EBSD Technique
  • Optimization of the Manufacturing Process of Sintered Fe-Mn-Cr-Mo-C Steels Using ANOVA
  • Direct Production of Tin Bronzes from Copper and Cassiterite
  • Microstructure-Properties Characterization of Selective Laser Melted Biomedical Co-28Cr-6Mo Alloy
  • Effect of Rare-Earth Doping on Dynamic Magnetic Properties of FeGa Alloy
  • Optimization of Raster Point Deposition Methodology for Deformation Analyses
  • Formation of Alpha-Case Layer during Oxidation of Ti6Al4V Surface by Annealing at 1050 °C and Change of Microstructure after Different Cooling Rates
  • Microstructure Analysis of Progressive Secondary AlSi7Mg0.6 Alloy with Higher Fe Content Using Electron Metallography Techniques
  • Comparison of Microstructure and Properties of Nickel-Copper Alloy Prepared by Casting and Laser Powder Bed Fusion Process
  • Formation of Sulphides in As-Cast GOES Thin Strips
  • Characterisation of a San Mai Steel Composite for the Manufacture of Knives
  • Numerical Simulation of the Welding Process during the Main Circulation Pump Impeller Repair
  • A Study of Cut Surface after the Abrasive Water Jet Application on the MS1 Material Prepared by DMLS Method
  • The Influence of Progressive Cladding Technologies on Layers Quality
  • Chapter 2: Corrosion
  • Identification of Corrosion Mechanisms of Stainless Steel with Metallography Cross Sections
  • Influence of Cavitation in Seawater on the Etching Attack of Manganese-Aluminum-Bronzes
  • Chapter 3: Fractographic Analysis
  • Microstructure and Fatigue Behavior of High-Performance Aluminum Alloy Al2024 Produced by Laser Powder Bed Fusion
  • Analysis of Cracks of Thermostats Casings Made of Brass
  • The Fractographic Analysis of Tensile and Fatigue Fracture Surfaces in Secondary A356 Aluminum Alloy with a Higher Concentration of Iron
  • Fracture Mechanisms of Austenitic Steel Caused by Dynamic Tests
  • High-Temperature Low Cycle Fatigue of Nickel-Based Superalloy IN738LC
  • Metallography of Fractured Aluminium Alloys for the Transmission System ́s Elements
  • Investigation of Fatigue Failure in Electric Locomotive Axle
  • Dynamic Fracture Characteristics of High-Strength Steel
  • Creep Resistance and Microstructure Evolution in HR3C-P92 Heterogeneous Welds
  • Analysis of Tribodegradation Factors Limiting the Life of the Molds
  • Chapter 4: Nanomaterials and Nanotechnologies
  • Preparation and Fracture Analysis of Advanced Layered Composite with Graphene-Coated Alumina Nanofibers
  • Influence of Ligands on Physicochemical Characteristics of Magnetic Nanoparticles
  • Carbon Fibers Doped by Binary Phosphides as an Electrocatalytic Layer for PEM Electrolysers
  • Chapter 5: Sample Preparation for Metallography
  • Evaluation of Sample Preparation Importance for Digital Image Correlation during Cold Deformation
  • Automation of Metallographic Sample Etching Process
Les mer

Produktdetaljer

ISBN
9783036400785
Publisert
2023-04-21
Utgiver
Vendor
Trans Tech Publications Ltd
Vekt
560 gr
Høyde
240 mm
Bredde
170 mm
Dybde
13 mm
Aldersnivå
P, 06
Språk
Product language
Engelsk
Format
Product format
Heftet
Antall sider
250